MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Loctite® Durabond® E-60HP Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes:
Epoxy Adhesives
Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific products designed to outperform the competition in all aspects: better adhesion, better flow, less odor, improved clarity, higher strength, and greater durability. All two-part Durabond® Structural Adhesives are packaged in easy-to-use, side-by-side cartridges for use with our manual dispensers and mix nozzles.

Loctite® E-60HP High strength, toughened, high peel, high shear Durabond® Epoxy Adhesive
A high strength epoxy with a 60-minute worklife. Off-white, toughened, high peel, high sheer.
  • Mix Ratio by Volume, Resin:Hardener = 2:1
Bonding Type: Epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 67500 cP67500 cPMixed - medium; Resin - 75,000 cP; Hardener - 7,000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Adhesive Bond Strength 20.7 - 34.5 MPa3000 - 5000 psiVaries with substrates
Peel Strength 3.51 - 12.3 kN/m20.0 - 70.0 pliVaries with substrates.
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 19.7 kV/mm500 kV/inTest run on 1/8" specimens.
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 60 min60 min
 
Descriptive Properties
ColorOff-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy)
Geon® Performance Solutions HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy)
Henkel Loctite® Durabond® E-30CL Epoxy Adhesive
Henkel Loctite® CHIPBONDER® 3615 High Adhesion, Syringe Dispense
Henkel Hysol EA 9377 Paste Adhesive System

PLOCT052 / 51788

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.