MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay CYCOM® 970 Epoxy - Carbon Fiber Reinforced Unidirectional Tape
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® 970 epoxy resin is a controlled flow, 350°F (177°C) curing epoxy resin with good 300°F (149°C) dry service capability. CYCOM 970 is excellent for producing nonporous, void-free honeycomb sandwich structures, as well as laminates. CYCOM 970 has adjustable tack and is available as unidirectional tape, fabric or roving. The prepreg is formulated for autoclave processing. Recommended cure is two hours at 350°F (177°C). No post-cure is required for dry service capability. The recommended lay-up procedure is L-9 for honeycomb core or L-8 for laminates. Recommended cure procedure is C-8. CYCOM 970 can be impregnated via solution technique on all available fibers and fabrics. Typical applications for CYCOM 970 include structural aircraft components requiring honeycomb sandwich panels.

Features & Benefits:

  • 350°F (177°C) cure
  • Available in a broad range of fibers and forms including tape, fabric and roving
  • Controlled flow resin for use in making honeycomb parts
  • 300°F (149°C) dry and 200°F (93°C) wet service temperature
  • Sandwich panel and laminate usage
  • Autoclave processing
  • Shelf life 6 months at 0°F (-18°C), 10 days at 72°F (22°C)
Applications: Structural aircraft components requiring honeycomb sandwich panels.

Property data for resin reinforced with Standard Modulus (33Msi/228 GPa Class) Carbon Fiber Reinforced Unidirectional Tape

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  4.37 - 4.70 MPa
@Temperature 93.0 °C
634 - 682 psi
@Temperature 199 °F
Flatwise
 4.81 - 5.19 MPa
@Temperature 24.0 °C
697 - 753 psi
@Temperature 75.2 °F
Flatwise
 1500 - 1720 MPa
@Temperature 93.0 °C
217000 - 249000 psi
@Temperature 199 °F
 1590 - 1760 MPa
@Temperature 24.0 °C
231000 - 255000 psi
@Temperature 75.2 °F
Tensile Modulus  119 - 120 GPa
@Temperature 93.0 °C
17300 - 17400 ksi
@Temperature 199 °F
 120 - 121 GPa
@Temperature 24.0 °C
17400 - 17500 ksi
@Temperature 75.2 °F
Compressive Strength  903 - 1027 MPa
@Temperature 93.0 °C
131000 - 149000 psi
@Temperature 199 °F
0° wet
 1117 - 1282 MPa
@Temperature 93.0 °C
162000 - 185900 psi
@Temperature 199 °F
 1323 - 1461 MPa
@Temperature 24.0 °C
191900 - 211900 psi
@Temperature 75.2 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °Fwet
 149 °C300 °Fdry
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 °C
@Time 7200 sec
350 °F
@Time 2.00 hour
Recommended Cure
Shelf Life  0.333 Month
@Temperature 22.2 °C
0.333 Month
@Temperature 72.0 °F
Resin
 6.00 Month
@Temperature -17.8 °C
6.00 Month
@Temperature 0.000 °F
Resin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman Araldite GY 281 Bisphenol F Epoxy Resin
Solvay CYCOM® 7714A Epoxy - Unidirectional Carbon Tape and Roving Composite
Solvay CYCOM® 5276-1 Epoxy with G40-800 Tape Composite
Overview of materials for Epoxy Adhesive
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage

PCYTED088 / 180390

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.