MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 970 Epoxy - Carbon Fiber Reinforced Unidirectional Tape
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® 970 epoxy resin is a controlled flow, 350°F (177°C) curing epoxy resin with good 300°F (149°C) dry service capability. CYCOM 970 is excellent for producing nonporous, void-free honeycomb sandwich structures, as well as laminates. CYCOM 970 has adjustable tack and is available as unidirectional tape, fabric or roving. The prepreg is formulated for autoclave processing. Recommended cure is two hours at 350°F (177°C). No post-cure is required for dry service capability. The recommended lay-up procedure is L-9 for honeycomb core or L-8 for laminates. Recommended cure procedure is C-8. CYCOM 970 can be impregnated via solution technique on all available fibers and fabrics. Typical applications for CYCOM 970 include structural aircraft components requiring honeycomb sandwich panels.

Features & Benefits:

  • 350°F (177°C) cure
  • Available in a broad range of fibers and forms including tape, fabric and roving
  • Controlled flow resin for use in making honeycomb parts
  • 300°F (149°C) dry and 200°F (93°C) wet service temperature
  • Sandwich panel and laminate usage
  • Autoclave processing
  • Shelf life 6 months at 0°F (-18°C), 10 days at 72°F (22°C)
Applications: Structural aircraft components requiring honeycomb sandwich panels.

Property data for resin reinforced with Standard Modulus (33Msi/228 GPa Class) Carbon Fiber Reinforced Unidirectional Tape

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 634 - 682 psi
@Temperature 93.0 °C
Flatwise
 697 - 753 psi
@Temperature 24.0 °C
Flatwise
 217000 - 249000 psi
@Temperature 93.0 °C
 231000 - 255000 psi
@Temperature 24.0 °C
Tensile Modulus 119 - 120 GPa
@Temperature 93.0 °C
 120 - 121 GPa
@Temperature 24.0 °C
Compressive Strength 903 - 1027 MPa
@Temperature 93.0 °C
0° wet
 1117 - 1282 MPa
@Temperature 93.0 °C
 1323 - 1461 MPa
@Temperature 24.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °Cwet
 149 °Cdry
 
Processing PropertiesOriginal ValueComments
Processing Temperature 350 °F
@Time 7200 sec
Recommended Cure
Shelf Life 0.333 Month
@Temperature 22.2 °C
Resin
 6.00 Month
@Temperature -17.8 °C
Resin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman Araldite GY 281 Bisphenol F Epoxy Resin
Solvay CYCOM® 7714A Epoxy - Unidirectional Carbon Tape and Roving Composite
Solvay CYCOM® 5276-1 Epoxy with G40-800 Tape Composite
Overview of materials for Epoxy Adhesive
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage

PCYTED088 / 180390

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.