MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kingfa PBT-RG151 Flame Retardant, 15% Glass Fiber Reinforced PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes:
    Features:
  • Flame retardant
  • High strength
  • High temperature properties
  • Good electric properties
  • Excellent size stability
  • No blooming

    Applications:
  • Injection molding
  • Connectors
  • Relay
  • Bobbins
  • Plugs
  • E & E parts

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.55 g/cc
@Temperature 23.0 °C
1.55 g/cc
@Temperature 73.4 °F
ASTM D792
Filler Content 15 %15 %Glass Fiber
Water Absorption 0.070 %
@Temperature 23.0 °C,
Time 86400 sec
0.070 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.011 cm/cm
@Temperature 23.0 °C
0.0050 - 0.011 in/in
@Temperature 73.4 °F
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength at Break 95.0 MPa13800 psi10mm/min; ASTM D638
Elongation at Break 3.4 %3.4 %10mm/min; ASTM D638
Flexural Strength 150 MPa21800 psi2mm/min; ASTM D790
Flexural Modulus 5.60 GPa812 ksi2mm/min; ASTM D790
Izod Impact, Notched 0.700 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.31 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
@Thickness 6.40 mm
419 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
@Thickness 6.40 mm
401 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94  V-0
@Thickness 0.300 mm
V-0
@Thickness 0.0118 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 265 °C<= 509 °F
Rear Barrel Temperature 220 - 240 °C428 - 464 °FStart Point: 235°C
Middle Barrel Temperature 235 - 255 °C455 - 491 °FStart Point: 245°C
Front Barrel Temperature 240 - 265 °C464 - 509 °FStart Point: 255°C
Melt Temperature 240 - 260 °C464 - 500 °FStart Point: 250°C
Mold Temperature 50.0 - 70.0 °C122 - 158 °FStart Point: 60°C
Drying Temperature 120 - 140 °C
@Time 14400 - 21600 sec
248 - 284 °F
@Time 4.00 - 6.00 hour
Pre-dry
 
Descriptive Properties
Injection SpeedModerate to High

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kingfa PBT-RG15 Flame Retardant, 15% Glass Fiber Reinforced PBT
Kingfa PBT-G15 15% Glass Fiber Reinforced PBT
Kingfa PA66-RG201 Flame Retardant, 20% Glass Fiber Reinforced PA66
Kingfa PA66-RG001 Flame Retardant PA66
Kingfa PBT-RG002 Flame Retardant PBT

PKINGF010 / 104269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.