MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kingfa PBT-RG151 Flame Retardant, 15% Glass Fiber Reinforced PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes:
    Features:
  • Flame retardant
  • High strength
  • High temperature properties
  • Good electric properties
  • Excellent size stability
  • No blooming

    Applications:
  • Injection molding
  • Connectors
  • Relay
  • Bobbins
  • Plugs
  • E & E parts

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.55 g/cc
@Temperature 23.0 °C
ASTM D792
Filler Content 15 %Glass Fiber
Water Absorption 0.070 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.011 cm/cm
@Temperature 23.0 °C
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength at Break 95.0 MPa10mm/min; ASTM D638
Elongation at Break 3.4 %10mm/min; ASTM D638
Flexural Strength 150 MPa2mm/min; ASTM D790
Flexural Modulus 5600 MPa2mm/min; ASTM D790
Izod Impact, Notched 70.0 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
@Thickness 6.40 mm
ASTM D648
Flammability, UL94 V-0
@Thickness 0.300 mm
 V-0
@Thickness 0.750 mm
 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 265 °C
Rear Barrel Temperature 220 - 240 °CStart Point: 235°C
Middle Barrel Temperature 235 - 255 °CStart Point: 245°C
Front Barrel Temperature 240 - 265 °CStart Point: 255°C
Melt Temperature 240 - 260 °CStart Point: 250°C
Mold Temperature 50.0 - 70.0 °CStart Point: 60°C
Drying Temperature 120 - 140 °C
@Time 14400 - 21600 sec
Pre-dry
 
Descriptive Properties
Injection SpeedModerate to High

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa PBT-RG15 Flame Retardant, 15% Glass Fiber Reinforced PBT
Kingfa PBT-G15 15% Glass Fiber Reinforced PBT
Kingfa PA66-RG201 Flame Retardant, 20% Glass Fiber Reinforced PA66
Kingfa PA66-RG001 Flame Retardant PA66
Kingfa PBT-RG002 Flame Retardant PBT

PKINGF010 / 104269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.