System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Kingfa PA66-RG001 Flame Retardant PA66
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Unreinforced, Flame Retardant
Material Notes:
Features:
Flame retardant
High strength
High temperature properties
Good electric properties
No blooming
Applications:
Injection molding
Connectors
Relay
Bobbins, plugs
E & E parts
Information Provided by Kingfa Sci. & Tech. Co., Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.26
g/cc
@Temperature 23.0 °C
1.26
g/cc
@Temperature 73.4 °F
ASTM D792
Water Absorption
0.60 %
@Temperature 23.0 °C,
Time 86400 sec
0.60 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage
0.012
-
0.014
cm/cm
@Temperature 23.0 °C
0.012
-
0.014
in/in
@Temperature 73.4 °F
ASTM D955
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
113
113
ASTM D785
Tensile Strength at Break
55.0
MPa
7980
psi
10mm/min; ASTM D638
Elongation at Break
>= 20 %
>= 20 %
10mm/min; ASTM D638
Flexural Strength
80.0
MPa
11600
psi
2mm/min; ASTM D790
Flexural Modulus
2.35
GPa
341
ksi
2mm/min; ASTM D790
Izod Impact, Notched
0.750
J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.41
ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+16
ohm-cm
1.00e+16
ohm-cm
ASTM D257
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
243
°C
@Thickness 6.40 mm
469
°F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
68.0
°C
@Thickness 6.40 mm
154
°F
@Thickness 0.252 in
ASTM D648
Flammability, UL94
V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Processing Properties
Metric
English
Comments
Processing Temperature
<=
310
°C
<=
590
°F
Rear Barrel Temperature
255
-
275
°C
491
-
527
°F
Start Point: 265°C
Middle Barrel Temperature
260
-
290
°C
500
-
554
°F
Start Point: 280°C
Front Barrel Temperature
270
-
300
°C
518
-
572
°F
Start Point: 285°C
Melt Temperature
275
-
300
°C
527
-
572
°F
Start Point: 285°C
Mold Temperature
50.0
-
70.0
°C
122
-
158
°F
Start Point: 60°C
Drying Temperature
90.0
-
110
°C
@Time 14400 - 21600 sec
194
-
230
°F
@Time 4.00 - 6.00 hour
Pre-dry
Descriptive Properties
Injection Speed
Moderate to High
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Kingfa PA66-RG201 Flame Retardant, 20% Glass Fiber Reinforced PA66
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant
Kingfa PA66-C111 Toughened PA66
Kingfa PA66-RG301 Flame Retardant, 30% Glass Fiber Reinforced PA66
Celanese Zytel® ST801 NC010A PA66-HI
PKINGF037 / 104296
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.