MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Resinlab® UR3001HP Black Urethane Encapsulant
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent environmental protection while having tenacious adhesion to various metals, plastics and other common assembly materials. UR3001HP Black is an unfilled system that has a gel-like Shore hardness and good flexibility at temperatures as low as –40°C. It provides excellent moisture resistance and can withstand 125°C continuous operation. UR3001HP Black has a convenient mixing ratio of 1 to 1 by volume. It is well suited to automated meter mix operations. UR3001HP Black is a DOT non-hazardous material and contains no TDI, MOCA, or other reportable substances. Part A is moisture sensitive and must be kept away from atmospheric moisture during storage. After opening a sealed container, thoroughly purge the remaining air space with dry nitrogen (or equivalent) before closing the container.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccPart B; TM R050-16
 1.07 g/cc1.07 g/ccMixed; TM R050-16
 1.15 g/cc1.15 g/ccPart A; TM R050-16
Water Absorption 0.31 %0.31 %30 days; TM R050-35
 0.21 %
@Time 259000 sec
0.21 %
@Time 72.0 hour
TM R050-35
Viscosity 100 cP100 cPPart A (Isocyanate), RVT, #2, 20 rpm; TM R050-12
 2000 cP2000 cPMixed; TM R050-12
 4000 cP4000 cPPart B (Polyol), RVT, #3, 20 rpm; TM R050-12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060TM R050-17
Tensile Strength at Break 0.0689 MPa10.0 psiTM R050-36
Tensile Strength, Ultimate 0.0689 MPa10.0 psiTM R050-36
Tensile Strength, Yield 0.0345 MPa5.00 psiTM R050-36
Elongation at Break 300 %300 %TM R050-36
Tensile Modulus 0.0000345 - 0.0000689 GPa0.00500 - 0.0100 ksiTM R050-36
Compressive Yield Strength 0.0345 - 0.0689 MPa5.00 - 10.0 psiTM R050-38
Compressive Strength 1.72 MPa250 psiUltimate; TM R050-38
 1.72 MPa250 psiBreak; TM R050-38
Compressive Modulus 0.000414 GPa0.0600 ksiTM R050-38
Adhesive Bond Strength 0.138 MPa20.0 psiLap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cm
Dielectric Constant 3.6
@Frequency 100 Hz,
Temperature 25.0 °C
3.6
@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 15.0 kV/mm380 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 µm/m-°C83.3 µin/in-°F
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg -66.0 °C-86.8 °FTM R050-25
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 85.0 °C
1.00 hour
@Temperature 185 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 15 - 20 min15 - 20 minMass: 50g; TM R050-19
 
Descriptive Properties
ColorBlack
Mix Ratio1:1Volume
 100:92Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Silica Aerogel
Overview of materials for Silicone Rubber
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Parker Chomerics Tecknit® 73-00008 Electrically Conductive Acrylic and Polyurethane Paint
Resinlab® UR3001HP Clear Urethane Encapsulant

PRESL188 / 101602

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.