MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics Tecknit® 73-00008 Electrically Conductive Acrylic and Polyurethane Paint
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosures, which are susceptible to EMI, and other applications requiring a flexible protective shield.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78 - 9278 - 92ASTM D2240
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.060 ohm<= 0.060 ohmCured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 161 °C322 °FCured
Minimum Service Temperature, Air -55.0 °C-67.0 °FCured
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 - 30200 min
@Temperature 24.0 °C
168 - 504 hour
@Temperature 75.2 °F
Pot Life 30 min
@Temperature 25.0 °C
30 min
@Temperature 77.0 °F
Shelf Life 9.00 Month9.00 MonthUnopened Container
 
Descriptive Properties
ColorGray
ConsistencyThin Paint
Coverage39 sq ftRecommended 0.002" thick
FillerAg
Final ConditionFlexible Film
Mix Ratio75.5:24.5
Number of ComponentsTwo
ResinPolyurethane
Volume11.4 in3
Weight12 oz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit® 72-00008 Silver-Filled Epoxy System
Overview of materials for Thermoset Polyurethane, Adhesive
Resinlab® UR3001HP Clear Urethane Encapsulant
Resinlab® UR3001HP Black Urethane Encapsulant
ITW Devcon Rubber Repair / Castable Urethane High Temp Edge & Seal (T-36), Amber

PCHOME413 / 131123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.