MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ITW Devcon Rubber Repair / Castable Urethane High Temp Edge & Seal (T-36), Amber
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes:

Information provided by ITW Devcon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0400 lb/in³
Viscosity 12000 cP12000 cPMixed Viscosity
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494Cured; ASTM D2240
Tensile Strength at Break 22.8 MPa3300 psiASTM D412
Elongation at Break <= 350 %<= 350 %ASTM D412
Tear Strength 90.3 kN/m515 pliASTM D624
Taber Abrasion, mg/1000 Cycles 8888H-18 wheel (1000 gram load)
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.8 kV/mm350 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °Fwet
 177 °C350 °Fdry
Shrinkage 0.14 %0.14 %Cured; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourFunctional cure
Pot Life 3.00 min
@Temperature 23.9 °C
3.00 min
@Temperature 75.0 °F
 
Descriptive Properties
Coverage per pound, in² @ 1/4" thickness100
Mix ratio by weight (Resin:Hardener)80:20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit® 73-00008 Electrically Conductive Acrylic and Polyurethane Paint
Resinlab® UR3001HP Clear Urethane Encapsulant
Resinlab® UR3001HP Black Urethane Encapsulant
Overview of materials for Thermoset Polyurethane, Adhesive

PITW10 / 48459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.