MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resinlab® UR3001HP Black Urethane Encapsulant
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent environmental protection while having tenacious adhesion to various metals, plastics and other common assembly materials. UR3001HP Black is an unfilled system that has a gel-like Shore hardness and good flexibility at temperatures as low as –40°C. It provides excellent moisture resistance and can withstand 125°C continuous operation. UR3001HP Black has a convenient mixing ratio of 1 to 1 by volume. It is well suited to automated meter mix operations. UR3001HP Black is a DOT non-hazardous material and contains no TDI, MOCA, or other reportable substances. Part A is moisture sensitive and must be kept away from atmospheric moisture during storage. After opening a sealed container, thoroughly purge the remaining air space with dry nitrogen (or equivalent) before closing the container.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccPart B; TM R050-16
 1.07 g/ccMixed; TM R050-16
 1.15 g/ccPart A; TM R050-16
Water Absorption 0.31 %30 days; TM R050-35
 0.21 %
@Time 259000 sec
TM R050-35
Viscosity 100 cPPart A (Isocyanate), RVT, #2, 20 rpm; TM R050-12
 2000 cPMixed; TM R050-12
 4000 cPPart B (Polyol), RVT, #3, 20 rpm; TM R050-12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60TM R050-17
Tensile Strength at Break 10.0 psiTM R050-36
Tensile Strength, Ultimate 10.0 psiTM R050-36
Tensile Strength, Yield 5.00 psiTM R050-36
Elongation at Break 300 %TM R050-36
Tensile Modulus 0.00500 - 0.0100 ksiTM R050-36
Compressive Yield Strength 5.00 - 10.0 psiTM R050-38
Compressive Strength 250 psiUltimate; TM R050-38
 250 psiBreak; TM R050-38
Compressive Modulus 0.0600 ksiTM R050-38
Adhesive Bond Strength 20.0 psiLap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
Dielectric Constant 3.6
@Frequency 100 Hz,
Temperature 25.0 °C
Dielectric Strength 380 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°C
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg -66.0 °CTM R050-25
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 85.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 15 - 20 minMass: 50g; TM R050-19
 
Descriptive Properties
ColorBlack
Mix Ratio1:1Volume
 100:92Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Silica Aerogel
Overview of materials for Silicone Rubber
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Parker Chomerics Tecknit® 73-00008 Electrically Conductive Acrylic and Polyurethane Paint
Resinlab® UR3001HP Clear Urethane Encapsulant

PRESL188 / 101602

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.