MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 1025 Steel, cold drawn, high temperature, stress relieved, 50-75 mm (2-3 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Machinability and weldability are fair. Cold formability of these steels is good to excellent. This grade responds favorably to heat treating and cold work.

Key Words: UNS G10250, AMS 5075, AMS 5077, ASTM A29, ASTM A510, ASTM A512, ASTM A519, ASTM A575, ASTM A576, FED QQ-S-700 (G10250), MIL-S-11310 (CS1025), MIL-S-7952, MIL-S-7952A, MIL-T-3520, MIL-T-5066, SAE J403, SAE J412, SAE J414, DIN 1.1158, JIS S 25 C, JIS S 28 C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.858 g/cc0.2839 lb/in³Chemical composition of 0.23% C, 0.635% Mn, 0.11% Si, annealed at 925°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 101101
Hardness, Knoop 119119Converted from Brinell
Hardness, Rockwell B 5858Converted from Brinell
Hardness, Vickers 104104Converted from Brinell
Tensile Strength, Ultimate 345 MPa50000 psi
Tensile Strength, Yield 275 MPa39900 psi
Elongation at Break 15 %15 %
Reduction of Area 40 %40 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000159 ohm-cm
@Temperature 0.000 °C
0.0000159 ohm-cm
@Temperature 32.0 °F
annealed specimen
 0.0000219 ohm-cm
@Temperature 100 °C
0.0000219 ohm-cm
@Temperature 212 °F
annealed specimen
 0.0000292 ohm-cm
@Temperature 200 °C
0.0000292 ohm-cm
@Temperature 392 °F
annealed specimen
 0.0000487 ohm-cm
@Temperature 400 °C
0.0000487 ohm-cm
@Temperature 752 °F
annealed specimen
 0.0000758 ohm-cm
@Temperature 600 °C
0.0000758 ohm-cm
@Temperature 1110 °F
annealed specimen
 0.0000925 ohm-cm
@Temperature 700 °C
0.0000925 ohm-cm
@Temperature 1290 °F
annealed specimen
 0.0001094 ohm-cm
@Temperature 800 °C
0.0001094 ohm-cm
@Temperature 1470 °F
annealed specimen
 0.0001136 ohm-cm
@Temperature 900 °C
0.0001136 ohm-cm
@Temperature 1650 °F
annealed specimen
 0.0001167 ohm-cm
@Temperature 1000 °C
0.0001167 ohm-cm
@Temperature 1830 °F
annealed specimen
 0.0001194 ohm-cm
@Temperature 1100 °C
0.0001194 ohm-cm
@Temperature 2010 °F
annealed specimen
 0.0001219 ohm-cm
@Temperature 1200 °C
0.0001219 ohm-cm
@Temperature 2190 °F
annealed specimen
 0.0001239 ohm-cm
@Temperature 1300 °C
0.0001239 ohm-cm
@Temperature 2370 °F
annealed specimen
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.1 µm/m-°C
@Temperature 20.0 - 100 °C
6.72 µin/in-°F
@Temperature 68.0 - 212 °F
 12.8 µm/m-°C
@Temperature 20.0 - 200 °C
7.11 µin/in-°F
@Temperature 68.0 - 392 °F
 13.3 µm/m-°C
@Temperature 20.0 - 300 °C
7.39 µin/in-°F
@Temperature 68.0 - 572 °F
 13.9 µm/m-°C
@Temperature 20.0 - 400 °C
7.72 µin/in-°F
@Temperature 68.0 - 752 °F
 14.4 µm/m-°C
@Temperature 20.0 - 500 °C
8.00 µin/in-°F
@Temperature 68.0 - 932 °F
 14.8 µm/m-°C
@Temperature 20.0 - 600 °C
8.22 µin/in-°F
@Temperature 68.0 - 1110 °F
Specific Heat Capacity  0.486 J/g-°C
@Temperature >=100 °C
0.116 BTU/lb-°F
@Temperature >=212 °F
annealed
 0.519 J/g-°C
@Temperature 150 - 200 °C
0.124 BTU/lb-°F
@Temperature 302 - 392 °F
 0.532 J/g-°C
@Temperature 200 - 250 °C
0.127 BTU/lb-°F
@Temperature 392 - 482 °F
 0.557 J/g-°C
@Temperature 250 - 300 °C
0.133 BTU/lb-°F
@Temperature 482 - 572 °F
 0.574 J/g-°C
@Temperature 300 - 350 °C
0.137 BTU/lb-°F
@Temperature 572 - 662 °F
 0.599 J/g-°C
@Temperature 350 - 400 °C
0.143 BTU/lb-°F
@Temperature 662 - 752 °F
 0.662 J/g-°C
@Temperature 450 - 500 °C
0.158 BTU/lb-°F
@Temperature 842 - 932 °F
 0.749 J/g-°C
@Temperature 550 - 600 °C
0.179 BTU/lb-°F
@Temperature 1020 - 1110 °F
 0.846 J/g-°C
@Temperature 650 - 700 °C
0.202 BTU/lb-°F
@Temperature 1200 - 1290 °F
 0.950 J/g-°C
@Temperature 750 - 800 °C
0.227 BTU/lb-°F
@Temperature 1380 - 1470 °F
 1.432 J/g-°C
@Temperature 700 - 750 °C
0.3423 BTU/lb-°F
@Temperature 1290 - 1380 °F
Thermal Conductivity 27.11 W/m-K188.1 BTU-in/hr-ft²-°F
 26.1 W/m-K
@Temperature 800 °C
181 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 31.8 W/m-K
@Temperature 700 °C
221 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 35.6 W/m-K
@Temperature 600 °C
247 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 39.4 W/m-K
@Temperature 500 °C
273 BTU-in/hr-ft²-°F
@Temperature 932 °F
 42.7 W/m-K
@Temperature 400 °C
296 BTU-in/hr-ft²-°F
@Temperature 752 °F
 46.0 W/m-K
@Temperature 300 °C
319 BTU-in/hr-ft²-°F
@Temperature 572 °F
 49.0 W/m-K
@Temperature 200 °C
340 BTU-in/hr-ft²-°F
@Temperature 392 °F
 51.2 W/m-K
@Temperature 100 °C
355 BTU-in/hr-ft²-°F
@Temperature 212 °F
 51.9 W/m-K
@Temperature 0.000 °C
360 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.22 - 0.28 %0.22 - 0.28 %
Iron, Fe 99.03 - 99.48 %99.03 - 99.48 %As remainder
Manganese, Mn 0.30 - 0.60 %0.30 - 0.60 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1025 Steel, cold drawn, high temperature, stress relieved, 32-50 mm (1.25-2 in) round
AISI 1025 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1025 Steel, as drawn, 50-75 mm (2-3 in) round
AISI 1025 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1025 Steel, as drawn, 16-22 mm (0.625-0.875 in) round

M1025K / 6887

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.