System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
ExxonMobil ESCOREZ™ 1102RM (Europe) Petroleum Hydrocarbon Resin
(discontinued **)
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
;
Polymer
;
Adhesive
Material Notes:
Aliphatic hydrocarbon resin specifically designed as a binder for thermoplastic road marking formulations.
Availability: Africa & Middle East and Europe
Information provided by ExxonMobil Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Brookfield Viscosity
1650
cP
@Temperature 160 °C
1650
cP
@Temperature 320 °F
ETM E-31
Molecular Weight
750
g/mol
750
g/mol
Mn; ETM E-83
Thermal Properties
Metric
English
Comments
Softening Point
97.8
°C
208
°F
ETM E-24
Glass Transition Temp, Tg
44.0
°C
111
°F
ETM E-90
Optical Properties
Metric
English
Comments
Yellow Index
35 %
35 %
Toluene solution with 50% resin in YI.; ETM E-13
Descriptive Properties
Thermal Color Stability
89 YI
5hr, 347F (175C), ETM E-15
Wax Cloud Point
148°C
(25/25/50), ETM E-10
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
ExxonMobil ESCOREZ™ 1102 (Americas) Petroleum Hydrocarbon Resin
Victrex APTIV™ 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled
SunChemical Gwent D2121102P1 UV Curable Dielectric Ink
Lotte Advanced Materials Infino® FD-1102 PC, FR
ExxonMobil ESCOREZ™ 5340 Petroleum Hydrocarbon Resin
PEXB492A / 138109
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.