MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil ESCOREZ™ 1102 (Americas) Petroleum Hydrocarbon Resin
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Adhesive

Material Notes: Aliphatic hydrocarbon resin which is designed for use in a varity of applicaitons.

Availability: Central America, North America and South America

Information provided by ExxonMobil Chemical

Key Words: Tackify, Tackifying Resin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1650 cP
@Temperature 160 °C
1650 cP
@Temperature 320 °F
ETM 22-31
Molecular Weight 1300 g/mol1300 g/molMn; ETM 300-83
 2900 g/mol2900 g/molMw; ETM 300-83
 
Thermal PropertiesMetricEnglishComments
Softening Point 100 °C212 °FETM 22-4
Glass Transition Temp, Tg 50.0 °C122 °FETM 300-90
 
Descriptive Properties
Color-Initial3.0 GETM 22-13
Thermal Color Stability12.0 G5 hr, 175°C, ETM 22-14
Wax Cloud Point110°CETM 22-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil ESCOREZ™ 1102RM (Europe) Petroleum Hydrocarbon Resin
ExxonMobil ESCOREZ™ 5340 Petroleum Hydrocarbon Resin
SunChemical Gwent D2121102P1 UV Curable Dielectric Ink
Lotte Advanced Materials Infino® FD-1102 PC, FR
ExxonMobil ESCOREZ™ 1315 Petroleum Hydrocarbon Resin

PEXB492 / 37797

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.