MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Sequel E3400-1 UV NAT Thermoplastic Olefinic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Sequel E3400-1 UV NAT fractional melt flow, high flexural modulus thermoplastic polyolefin (TPO) is typically used for thermoformed exterior or interior applications that require low-temperature toughness and dimensional stability. This extrusion-grade material exhibits enhanced melt strength for a wide thermoforming processing window. Applications: Industrial, Panels & Profiles

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183-1
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.60 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.0 MPa3050 psi50mm/min; ISO 527-1,-2
Flexural Modulus 2.00 GPa290 ksi2mm/min; ISO 178
Impact Test 24.0 J
@Temperature -15.0 °C
17.7 ft-lb
@Temperature 5.00 °F
Multi-axial Impact Strength, 2.2m/s, 3.2mm plaque, energy @ peak force; material exhibits ductile behavior; ASTM D 3763
 
Descriptive Properties
Processing MethodExtrusion Flat-die, Thermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Sequel E3400 UV NAT Thermoplastic Olefinic Elastomer
Solvay Engineered Polymers Dexflex® E-300 TPO, Extrusion Grade
SEKISUI SPI ALLEN® E3400 TPO
Sandvik 3R60 (Urea Grade) Seamless tube and pipe
LyondellBasell SEQUEL® E3000 TPO

PEQT8773 / 220407

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.