Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion-grade material is readily processed into a variety of products and has excellent chemical resistance. This material can be supplied with or without UV stabilizers. Applications: Sheet extrusion and thermoforming Information provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay Engineered Polymers in 2008. |