MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 3R60 (Urea Grade) Seamless tube and pipe
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Sandvik 3R60 Urea Grade is a high-purity variant of AISI 316L, especially developed for the urea industry. The steel grade has a guaranteed maximum ferrite content of 0.6%. The characteristics of Sandvik 3R60 Urea Grade are:
  • high resistance to corrosion in ammonium carbamate
  • high resistance to intergranular corrosion
  • good weldability
  • Information provided by Sandvik

    ASTM 316L; UNS S31603; EN 1.4435

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 8.00 g/cc0.289 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell B <= 90<= 90
    Tensile Strength, Ultimate 490 - 690 MPa71100 - 100000 psi
     >= 390 MPa
    @Temperature 400 °C
    >= 56600 psi
    @Temperature 752 °F
     >= 415 MPa
    @Temperature 200 °C
    >= 60200 psi
    @Temperature 392 °F
    Tensile Strength, Yield  >= 190 MPa
    @Strain 0.2 %
    >= 27600 psi
    @Strain 0.2 %
     >= 235 MPa
    @Strain 1 %
    >= 34100 psi
    @Strain 1 %
     >= 110 MPa
    @Strain 0.2 %,
    Temperature 400 °C
    >= 16000 psi
    @Strain 0.2 %,
    Temperature 752 °F
     >= 115 MPa
    @Strain 0.2 %,
    Temperature 350 °C
    >= 16700 psi
    @Strain 0.2 %,
    Temperature 662 °F
     >= 120 MPa
    @Strain 0.2 %,
    Temperature 300 °C
    >= 17400 psi
    @Strain 0.2 %,
    Temperature 572 °F
     >= 130 MPa
    @Strain 0.2 %,
    Temperature 250 °C
    >= 18900 psi
    @Strain 0.2 %,
    Temperature 482 °F
     >= 135 MPa
    @Strain 1 %,
    Temperature 400 °C
    >= 19600 psi
    @Strain 1 %,
    Temperature 752 °F
     >= 140 MPa
    @Strain 0.2 %,
    Temperature 200 °C
    >= 20300 psi
    @Strain 0.2 %,
    Temperature 392 °F
     >= 140 MPa
    @Strain 1 %,
    Temperature 350 °C
    >= 20300 psi
    @Strain 1 %,
    Temperature 662 °F
     >= 145 MPa
    @Strain 1 %,
    Temperature 300 °C
    >= 21000 psi
    @Strain 1 %,
    Temperature 572 °F
     >= 150 MPa
    @Strain 0.2 %,
    Temperature 150 °C
    >= 21800 psi
    @Strain 0.2 %,
    Temperature 302 °F
     >= 155 MPa
    @Strain 1 %,
    Temperature 250 °C
    >= 22500 psi
    @Strain 1 %,
    Temperature 482 °F
     >= 165 MPa
    @Strain 0.2 %,
    Temperature 100 °C
    >= 23900 psi
    @Strain 0.2 %,
    Temperature 212 °F
     >= 165 MPa
    @Strain 1 %,
    Temperature 200 °C
    >= 23900 psi
    @Strain 1 %,
    Temperature 392 °F
     >= 180 MPa
    @Strain 1 %,
    Temperature 150 °C
    >= 26100 psi
    @Strain 1 %,
    Temperature 302 °F
     >= 180 MPa
    @Strain 0.2 %,
    Temperature 50.0 °C
    >= 26100 psi
    @Strain 0.2 %,
    Temperature 122 °F
     >= 225 MPa
    @Strain 1 %,
    Temperature 50.0 °C
    >= 32600 psi
    @Strain 1 %,
    Temperature 122 °F
     >= 300 MPa
    @Strain 1 %,
    Temperature 100 °C
    >= 43500 psi
    @Strain 1 %,
    Temperature 212 °F
    Elongation at Break >= 40 %>= 40 %
    Modulus of Elasticity 200 GPa29000 ksi
     165 GPa
    @Temperature 500 °C
    23900 ksi
    @Temperature 932 °F
     172 GPa
    @Temperature 400 °C
    24900 ksi
    @Temperature 752 °F
     179 GPa
    @Temperature 300 °C
    26000 ksi
    @Temperature 572 °F
     186 GPa
    @Temperature 200 °C
    27000 ksi
    @Temperature 392 °F
     194 GPa
    @Temperature 100 °C
    28100 ksi
    @Temperature 212 °F
    Charpy Impact >= 149 J
    @Temperature -60.0 °C
    >= 110 ft-lb
    @Temperature -76.0 °F
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  16.5 µm/m-°C
    @Temperature 30.0 - 100 °C
    9.17 µin/in-°F
    @Temperature 86.0 - 212 °F
     17.0 µm/m-°C
    @Temperature 30.0 - 200 °C
    9.44 µin/in-°F
    @Temperature 86.0 - 392 °F
     17.5 µm/m-°C
    @Temperature 30.0 - 300 °C
    9.72 µin/in-°F
    @Temperature 86.0 - 572 °F
     18.0 µm/m-°C
    @Temperature 30.0 - 400 °C
    10.0 µin/in-°F
    @Temperature 86.0 - 752 °F
     18.0 µm/m-°C
    @Temperature 30.0 - 500 °C
    10.0 µin/in-°F
    @Temperature 86.0 - 932 °F
     18.5 µm/m-°C
    @Temperature 30.0 - 700 °C
    10.3 µin/in-°F
    @Temperature 86.0 - 1290 °F
     33.3 µm/m-°C
    @Temperature 30.0 - 600 °C
    18.5 µin/in-°F
    @Temperature 86.0 - 1110 °F
    Specific Heat Capacity  0.485 J/g-°C
    @Temperature 20.0 °C
    0.116 BTU/lb-°F
    @Temperature 68.0 °F
     0.500 J/g-°C
    @Temperature 100 °C
    0.120 BTU/lb-°F
    @Temperature 212 °F
     0.515 J/g-°C
    @Temperature 200 °C
    0.123 BTU/lb-°F
    @Temperature 392 °F
     0.525 J/g-°C
    @Temperature 300 °C
    0.125 BTU/lb-°F
    @Temperature 572 °F
     0.540 J/g-°C
    @Temperature 400 °C
    0.129 BTU/lb-°F
    @Temperature 752 °F
     0.555 J/g-°C
    @Temperature 500 °C
    0.133 BTU/lb-°F
    @Temperature 932 °F
     0.575 J/g-°C
    @Temperature 600 °C
    0.137 BTU/lb-°F
    @Temperature 1110 °F
    Thermal Conductivity  14.0 W/m-K
    @Temperature 20.0 °C
    97.2 BTU-in/hr-ft²-°F
    @Temperature 68.0 °F
     15.0 W/m-K
    @Temperature 100 °C
    104 BTU-in/hr-ft²-°F
    @Temperature 212 °F
     17.0 W/m-K
    @Temperature 200 °C
    118 BTU-in/hr-ft²-°F
    @Temperature 392 °F
     18.0 W/m-K
    @Temperature 300 °C
    125 BTU-in/hr-ft²-°F
    @Temperature 572 °F
     20.0 W/m-K
    @Temperature 400 °C
    139 BTU-in/hr-ft²-°F
    @Temperature 752 °F
     21.0 W/m-K
    @Temperature 500 °C
    146 BTU-in/hr-ft²-°F
    @Temperature 932 °F
     23.0 W/m-K
    @Temperature 600 °C
    160 BTU-in/hr-ft²-°F
    @Temperature 1110 °F
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C <= 0.020 %<= 0.020 %
    Chromium, Cr 17.5 %17.5 %
    Iron, Fe 63.8 %63.8 %As Balance
    Manganese, Mn 1.7 %1.7 %
    Molybdenum, Mo 2.6 %2.6 %
    Nickel, Ni 14 %14 %
    Phosphorus, P <= 0.015 %<= 0.015 %
    Silicon, Si 0.40 %0.40 %
    Sulfur, S <= 0.010 %<= 0.010 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants
    AISI Type 316L Stainless Steel, annealed bar
    Aluminum 5005-O
    Aurora Plastics G-4275E Extrusion Compound
    Solvay Engineered Polymers Dexflex® E-300 TPO, Extrusion Grade

    NSANDV234 / 19128

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.