MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek REDLINE MULTIKOTE Water-Based Coating
Categories: Ceramic

Material Notes: A water-based coating designed to prevent molten metal adhesion to both refractory and most metallic surfaces. Multikote's bonding system enables it to be applied in a variety of applications including both hand and automatic ladles, thermocouple tubes, sow molds, troughs, casting tables, most boards, flooring, and other surfaces which require a protective coating. Stainless steel requires wire brush or acid prep.

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point -6.67 °C20.0 °FBefore application
Maximum Service Temperature, Air 1649 °C3000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast XL Small Component Refractory
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Pyrotek Pyromoldable JDR1150A Moldable Paste Type Low Density Refractory
Pyrotek Pyromat TS-045 Electrical Insulating Board
Pyrotek Pyrocast ZS Refractory Shapes

CPYRO201 / 1918

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.