MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Pyromat TS-045 Electrical Insulating Board
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: Pyromat TS-045 is a black laminate, press molded from high-temperature thermoset resin and reinforced with glass filament mat. Its composition ensures excellent chemically resistance and antistatic properties. Each board is surface ground to achieve accurate dimensions on thickness and parallelism. Pyromat TS-045 is specifically formulated to provide optimum properties for the manufacture of solder pallets for the PCB industry.

Applications

  • Wave solder pallet / carrier support

Advantages

  • Superior antistatic properties
  • Excellent chemical durability
  • Exceptional thermal resistance
  • Superior parallelism and flatness
  • Good machining characteristics
  • Easy to wash and handle
  • Dimensionally stable

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 - 1.90 g/cc0.0650 - 0.0686 lb/in³
Water Absorption <= 0.18 %<= 0.18 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 400 MPa58000 psi
Compressive Strength 500 MPa72500 psi
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+6 - 1.00e+10 ohm1.00e+6 - 1.00e+10 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °FContinuous
 300 °C572 °FIntermittent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrotek Pyrocast XL Small Component Refractory
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass

PPYRO166 / 58411

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.