MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Categories: Carbon; Graphite

Material Notes: S-679 is an isostatically pressed graphite material that is treated to provide oxidation resistance at elevated temperatures. This material performs well in glass contact applications where heat and abrasion cause other materials to fail.

Applications

  • Take out tongs
  • Dead plates
  • Sweep out inserts
  • Stacker bar covers
  • Conveyor guides
  • Transfer units
  • Precision machined parts
  • Rollers

Advantages

  • Asbestos-free
  • Uniform heat distribution
  • Non-sticking to glass
  • Low heat capacity
  • Long life
  • Compatible in combination with steel or other metals

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.842 g/cc0.06655 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 68.9 MPa9990 psi
Compressive Strength 144.8 MPa21000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.70 µm/m-°C
@Temperature 21.0 - 982 °C
1.50 µin/in-°F
@Temperature 69.8 - 1800 °F
Thermal Conductivity 45.0 W/m-K312 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 649 °C1200 °FContinuous use
 1288 °C2350 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes
Poco Graphite POCOFoam® Graphite Foam
Momentive Performance Materials Pyrolytic Graphite (PG) Coating
Graphite, Carbon, C
Momentive Performance Materials "PG" Pyrolytic Graphite

CPYRO084 / 1822

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.