MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom ZB 752 AC T 2065 (EBONY) Polypropylene, Talc Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Hostacom ZB 752 AC T 2065 is a talc filled PP homopolymer, with medium melt flow rate, good stiffness, and good thermal resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 2065 color version. Applications: Automotive Parts, Under hood

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183-1A
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.0 MPa4640 psiISO 527-1,-2
Flexural Modulus 2.80 GPa406 ksiISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C244 °Funannealed; ISO 75B-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °Funannealed; ISO 75A-1,-2
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom™ ZB752AC Polypropylene Homopolymer
LyondellBasell Hostacom X M3 N07 105555 Polypropylene with 30% Talc Filler
LyondellBasell Hostacom Hostacom HYP 376D NAT Polypropylene, Mineral Reinforced
LyondellBasell Hostacom 1103 NATURAL Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 2-2120 20% Talc-Filled Polypropylene Block-Copolymer

PEQT8440 / 220075

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.