MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom Hostacom HYP 376D NAT Polypropylene, Mineral Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Hostacom HYP 376D NAT is a mineral filled PP homopolymer with very high melt flow rate. Applications: White Goods

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183-1A
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash 45.5 %
@Treatment Temp. 500 °C
45.5 %
@Treatment Temp. 932 °F
ISO 3451-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psiISO 527-1,-2
Elongation at Yield 3.0 %3.0 %ISO 527-1,-2
Tensile Modulus 2.70 GPa392 ksiISO 527-1,-2
Flexural Modulus 2.80 GPa406 ksiTech.A; ISO 178/A1
Charpy Impact Unnotched  2.40 J/cm²
@Temperature 0.000 °C
11.4 ft-lb/in²
@Temperature 32.0 °F
ISO 179-1/1eU
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eU
Charpy Impact, Notched  0.150 J/cm²
@Temperature 0.000 °C
0.714 ft-lb/in²
@Temperature 32.0 °F
ISO 179-1/1eA
 0.220 J/cm²
@Temperature 23.0 °C
1.05 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C207 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C135 °FISO 75-1,-2
Vicat Softening Point 93.0 °C199 °FB50N; ISO 306
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis PS65T20 Polypropylene Compound, Mineral Filled
Celanese SO.F.TER Talcoprene® C340TC Talc-Reinforced Polypropylene
Inno-Comp INNOPOL® CS 2-2120 20% Talc-Filled Polypropylene Block-Copolymer
LyondellBasell Hostacom X M3 N07 105555 Polypropylene with 30% Talc Filler
LyondellBasell Hostacom 1103 NATURAL Polypropylene with 20% Talc Filler

PEQT8003 / 219639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.