Hostacom ZB 752 AC T 2065 is a talc filled PP homopolymer, with medium melt flow rate, good stiffness, and good thermal resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 2065 color version. Applications: Automotive Parts, Under hoodInformation provided by LyondellBasell. |