MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A227M Steel Wire, Class I
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Round, hard drawn steel wire for mechanical springs and wire forms

Key Words: UNS K06501
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Typical of ASTM Steel
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1010 - 1170 MPa
@Diameter 16.0 mm
146000 - 170000 psi
@Diameter 0.630 in
 1070 - 1240 MPa
@Diameter 13.0 mm
155000 - 180000 psi
@Diameter 0.512 in
 1130 - 1310 MPa
@Diameter 10.0 mm
164000 - 190000 psi
@Diameter 0.394 in
 1190 - 1370 MPa
@Diameter 8.00 mm
173000 - 199000 psi
@Diameter 0.315 in
 1220 - 1410 MPa
@Diameter 7.00 mm
177000 - 205000 psi
@Diameter 0.276 in
 1280 - 1470 MPa
@Diameter 6.00 mm
186000 - 213000 psi
@Diameter 0.236 in
 1320 - 1510 MPa
@Diameter 5.00 mm
191000 - 219000 psi
@Diameter 0.197 in
 1380 - 1590 MPa
@Diameter 4.00 mm
200000 - 231000 psi
@Diameter 0.157 in
 1460 - 1680 MPa
@Diameter 3.00 mm
212000 - 244000 psi
@Diameter 0.118 in
 1580 - 1810 MPa
@Diameter 2.00 mm
229000 - 263000 psi
@Diameter 0.0787 in
 1640 - 1880 MPa
@Diameter 1.60 mm
238000 - 273000 psi
@Diameter 0.0630 in
 1770 - 2040 MPa
@Diameter 1.00 mm
257000 - 296000 psi
@Diameter 0.0394 in
 1830 - 2100 MPa
@Diameter 0.800 mm
265000 - 305000 psi
@Diameter 0.0315 in
 1870 - 2140 MPa
@Diameter 0.700 mm
271000 - 310000 psi
@Diameter 0.0276 in
 1920 - 2200 MPa
@Diameter 0.600 mm
278000 - 319000 psi
@Diameter 0.0236 in
 1960 - 2240 MPa
@Diameter 0.500 mm
284000 - 325000 psi
@Diameter 0.0197 in
Modulus of Elasticity 200 GPa29000 ksiTypical Carbon Steel
Bulk Modulus 160 GPa23200 ksiTypical for Steel
Poissons Ratio 0.290.29Typical Carbon Steel
Shear Modulus 80.0 GPa11600 ksiTypical for Steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cmTypical Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C6.67 µin/in-°FTypical Carbon Steel
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°FTypical Carbon Steel
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°FTypical Carbon Steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.45 - 0.85 %0.45 - 0.85 %may not vary by more than .13% in any one lot
Iron, Fe 98.255 %98.255 %as balance
Manganese, Mn 0.30 - 1.3 %0.30 - 1.3 %may not vary by more than .30% in any one lot
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A227 Steel Wire, Class II
ASTM A227M Steel Wire, Class II
ASTM A227 Steel Wire, Class I
ASTM A229 Oil-tempered Steel Wire, Class I
ASTM A229 Oil-tempered Steel Wire, Class II

MSA227MI / 142766

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.