MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Kanthal SW 821 Spray Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: KANTHAL SW 821 is a copper-nickel alloy wire developed for use in Arc and Flame Spray systems. The wire produces dense, well bonding coatings. The coatings are resistant against corrosion, typically used in marine and certain chemical applications.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 626 MPa90800 psi
Tensile Strength, Yield 577 MPa
@Strain 0.2 %
83700 psi
@Strain 0.2 %
Elongation at Break 8.0 %8.0 %
Modulus of Elasticity 178 GPa25800 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 1350 °C2460 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 32.75 %>= 32.75 %
Iron, Fe <= 2.5 %<= 2.5 %
Manganese, Mn <= 1.25 %<= 1.25 %
Nickel, Ni >= 63 %>= 63 %
Silicon, Si <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Kanthal D Resistance Ribbon
Sandvik Kanthal SW 010 Spray Wire
Sandvik Kanthal D Resistance Wire
Sandvik Kanthal APM Resistance Wire
Sandvik Kanthal AE Resistance Wire

NSANDV263 / 19157

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.