MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, HTA
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Fiber Designation: C193PW, Plain weave

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 49.5 %49.5 %Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 940 MPa
@Temperature 23.0 °C
136000 psi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Tensile Modulus 57.0 GPa
@Temperature 23.0 °C
8270 ksi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Flexural Yield Strength  672 MPa
@Temperature 90.0 °C
97500 psi
@Temperature 194 °F
0°, Conditioning: 23°C; ASTM D790
 946 MPa
@Temperature 23.0 °C
137000 psi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D790
Flexural Modulus  37.0 GPa
@Temperature 90.0 °C
5370 ksi
@Temperature 194 °F
0°, Conditioning: 23°C; ASTM D790
 40.0 GPa
@Temperature 23.0 °C
5800 ksi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D790
Compressive Yield Strength  419 MPa
@Temperature 90.0 °C
60800 psi
@Temperature 194 °F
0°, Conditioning: 23°C; ASTM D965
 592 MPa
@Temperature 23.0 °C
85900 psi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D965
Shear Strength  40.0 MPa
@Temperature 60.0 °C
5800 psi
@Temperature 140 °F
0°, Interlaminar, Conditioning: 60°C-90% RH; ASTM D2344
 43.0 MPa
@Temperature 90.0 °C
6240 psi
@Temperature 194 °F
0°, Interlaminar, Conditioning: 23°C; ASTM D2344
 66.0 MPa
@Temperature 23.0 °C
9570 psi
@Temperature 73.4 °F
0°, Interlaminar, Conditioning: 23°C; ASTM D2344
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
Dry Resin Content (%)42

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® M10E Epoxy Resin
Hexcel® HexPly® F593 Epoxy Resin
Hexcel® HexPly® F522 Epoxy Resin
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix

PHEXC197 / 98668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.