MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, HTA
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Fiber Designation: C193PW, Plain weave

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 49.5 %Fiber Volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 940 MPa
@Temperature 23.0 °C
0°, Conditioning: 23°C; ASTM D3039
Tensile Modulus 57.0 GPa
@Temperature 23.0 °C
0°, Conditioning: 23°C; ASTM D3039
Flexural Yield Strength 672 MPa
@Temperature 90.0 °C
0°, Conditioning: 23°C; ASTM D790
 946 MPa
@Temperature 23.0 °C
0°, Conditioning: 23°C; ASTM D790
Flexural Modulus 37.0 GPa
@Temperature 90.0 °C
0°, Conditioning: 23°C; ASTM D790
 40.0 GPa
@Temperature 23.0 °C
0°, Conditioning: 23°C; ASTM D790
Compressive Yield Strength 419 MPa
@Temperature 90.0 °C
0°, Conditioning: 23°C; ASTM D965
 592 MPa
@Temperature 23.0 °C
0°, Conditioning: 23°C; ASTM D965
Shear Strength 40.0 MPa
@Temperature 60.0 °C
0°, Interlaminar, Conditioning: 60°C-90% RH; ASTM D2344
 43.0 MPa
@Temperature 90.0 °C
0°, Interlaminar, Conditioning: 23°C; ASTM D2344
 66.0 MPa
@Temperature 23.0 °C
0°, Interlaminar, Conditioning: 23°C; ASTM D2344
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
Dry Resin Content (%)42

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® M10E Epoxy Resin
Hexcel® HexPly® F593 Epoxy Resin
Hexcel® HexPly® F522 Epoxy Resin
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix

PHEXC197 / 98668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.