MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyurethane, TP

Material Notes: PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding applications. This natural TPU resin features properties similar to standard TPU of same hardness (i.e. excellent mechanical properties and abrasion resistance)

Applications: PEARLTHANE® ECO D12T90E enhances the performance of a wide range of end use products that ranges from automotive, consumer electronics and sport and leisure applications among others where environmentally-friendly materials can bring value to the end product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ISO 868
Tensile Strength 37.99 MPa5510 psiISO 527-2/5A/500
Tensile Stress at Strain  9.03 MPa
@Strain 100 %
1310 psi
@Strain 100 %
ISO 527-2/5A/500
 25.03 MPa
@Strain 300 %
3630 psi
@Strain 300 %
ISO 527-2/5A/500
Elongation at Break 470 %470 %ISO 527-2/5A/500
Tear Strength 122 kN/m696 pliDie C; ISO 34-1B
Abrasion 3535mm3 Loss; ISO 4649
 
Processing PropertiesMetricEnglishComments
Zone 1 190 - 200 °C374 - 392 °F
Zone 2 195 - 205 °C383 - 401 °F
Zone 3 200 - 210 °C392 - 410 °F
Zone 4 200 - 210 °C392 - 410 °F
Adapter Temperature 205 - 215 °C401 - 419 °F5
Die Temperature 200 °C392 °FTIP (7)
 205 °C401 °F(6)
Drying Temperature 80.0 °C
@Time 10800 sec
176 °F
@Time 3.00 hour
Dew Point <= -30.0 °C<= -22.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer

PMEQU969a / 159335

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.