MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Synres® SR 1288A Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection molded siding panels, pool products, transportation parts, various home products as well as other applications requiring higher rigidity, lower shrinkage and lower coefficient of linear thermal expansion than natural polyolefins. These compounds can be tailored to specific needs and are available pre-colored or natural.

Forms: Pellets

Information Provided by Teknor Apex

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 606010 seconds; ASTM D2240
Tensile Strength at Break 26.2 MPa3800 psiASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus 1.90 GPa275 ksiASTM D790
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen EP200R Injection Molding Grade Polypropylene
Phillips Sumika Marlex® ALN-230 Polypropylene Impact Copolymer
LyondellBasell Moplen EP200R Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Astryn EPF30U Polypropylene Copolymer
ExxonMobil PP7043L1 Polypropylene Impact Copolymer

PTEKNO819 / 129000

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.