MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Moplen EP200R Polypropylene, Impact Modified; Molded/Extruded  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Moplen EP200R is a "Reactor-made Thermoplastic PolyOlefin", super impact copolymer with high impact resistance. Typical customer application is compounding base resin for automotive bumper fascia. Applications: Exterior Automotive Applications, Interior Automotive Applications

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 21 g/10 min
@Load 2.16 kg,
Temperature 230 °C
21 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 5050ASTM D785
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Yield 18.0 MPa2610 psiASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Modulus 0.750 GPa109 ksiASTM D790
Izod Impact, Notched  1.30 J/cm
@Temperature -20.0 °C
2.44 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648
Vicat Softening Point 130 °C266 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 30 %30 %ASTM D523
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Synres® SR 1288A Polypropylene
PolyMirae Moplen EP200R Injection Molding Grade Polypropylene
Phillips Sumika Marlex® ALN-230 Polypropylene Impact Copolymer
LyondellBasell Astryn EPF30U Polypropylene Copolymer
ExxonMobil PP7043L1 Polypropylene Impact Copolymer

PEQT8896 / 220530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.