MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Moplen EP200R Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Moplen EP200R is the reactor TPO manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP200R is a super impact copolymer particularly suitable for injection molding of high impact resistance required application and compounding base resin of automotive bumper fascia.

Features: Super high impact strength even at low temperature; Improved processability

Applications: Automotive; High impact resistance required application; Container

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 21 g/10 min
@Load 2.16 kg,
Temperature 230 °C
21 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 5050ASTM D785
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Yield 17.7 MPa2560 psiASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Modulus 0.735 GPa107 ksiASTM D790
Izod Impact, Notched  1.27 J/cm
@Temperature -20.0 °C
2.39 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648
Vicat Softening Point 130 °C266 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 30 %30 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Synres® SR 1288A Polypropylene
Phillips Sumika Marlex® ALN-230 Polypropylene Impact Copolymer
LyondellBasell Moplen EP200R Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Astryn EPF30U Polypropylene Copolymer
ExxonMobil PP7043L1 Polypropylene Impact Copolymer

PMIRAE02 / 53114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.