System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Epoxy Technology EPO-TEK® H81A Epoxy
Categories:
Polymer
;
Thermoset
;
Epoxy
Material Notes:
Material Description: A two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.
Information Provided by Epoxy Technology
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
5.62
g/cc
5.62
g/cc
Part B
5.80
g/cc
5.80
g/cc
Part A
Particle Size
<=
50
µm
<=
50
µm
Viscosity
250000
-
300000
cP
@Temperature 23.0 °C
250000
-
300000
cP
@Temperature 73.4 °F
0.5 rpm
Mechanical Properties
Metric
English
Comments
Shear Strength
>=
11.7
MPa
>=
1700
psi
Die
Electrical Properties
Metric
English
Comments
Volume Resistivity
<=
0.00090
ohm-cm
<=
0.00090
ohm-cm
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
250
°C
482
°F
Continuous
350
°C
662
°F
Intermittent
Minimum Service Temperature, Air
-55.0
°C
-67.0
°F
Continuous
-55.0
°C
-67.0
°F
Intermittent
Glass Transition Temp, Tg
>=
100
°C
>=
212
°F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature
412
°C
774
°F
Degradation Temperature
Processing Properties
Metric
English
Comments
Cure Time
60.0
min
@Temperature 150 °C
1.00
hour
@Temperature 302 °F
Minimum
Pot Life
2880
min
2880
min
Shelf Life
12.0
Month
@Temperature 25.0 °C
12.0
Month
@Temperature 77.0 °F
Descriptive Properties
Color
Dark Brown
Part A
Dark Brown
Part B
Consistency
Thick paste
Mix Ratio by Weight
6:1
Number of Components
Two
Weight Loss
<0.5%
200°C
0.07%
250°C
0.16%
300°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 310M-T Flexible Epoxy
Epoxy Technology EPO-TEK® 430 Epoxy
Epoxy Technology EPO-TEK® H31D-LV Epoxy
Epoxy Technology EPO-TEK® H55 Epoxy
Epoxy Technology EPO-TEK® EE149-6 Epoxy
PPOXYT049 / 141088
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.