MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Standex Engraving Tribocoat® Electroless Nickel Teflon Mold Coating
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Nickel Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Electroless Nickel with 25% PTFE. Tribocoat® is a proven composite electroless coating that has a superior combination of corrosion resistance, wear resistance, dry lubrication, and adhesion properties. It will coat tool steels, BeCu, forged aluminum, cast iron, and stainless steels. When used as a mold coating in the plastics processing industry, it reduces cycle time, gives quick effortless release, resists corrosion, and extends mold life.

Information provided by Mold-Tech®, Standex Engraving Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 0.200 - 2.00 microns0.00787 - 0.0787 mil+/- 0.1 micron uniformity across all coated surfaces
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 32 - 4532 - 45depends on application
Coefficient of Friction 0.100.10
Taber Abrasion, mg/1000 Cycles 1414CS-10 wheel; 1 kg load
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 354 °C670 °F
Minimum Service Temperature, Air -45.6 °C-50.0 °F
 
Component Elements PropertiesMetricEnglishComments
Nickel, Ni 75 %75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
Chemours Teflon® PTFE 7A Granular Molding Powder
Titanium Ti-6Al-4V (Grade 5), Annealed
Overview of materials for Nylon 66, Unreinforced
Nitinol - NiTi Shape Memory Alloy; High-Temperature Phase

NMOLDT00 / 18442

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.