MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: RADEL® R is a Polyphenylsulfone produced by Solvay Advanced Polymers. RADEL® R is in the same performance category as products like Polysulfone and ULTEM® (PEI). RADEL® R has increased performance versus Polysulfone and ULTEM® in terms of temperature, impact strength and chemical resistance. RADEL® R has exceptional resistance to repeated steam autoclaving without loss of dimensional stability or physical properties. RADEL® R comes in both opaque and transparent grades. The transparent grade is R-5500 and the opaque grade is R-5100.

  • High tensile strength
  • Excellent heat resistance
  • Very high resistance to environmental stress
  • Great mechanical strength
  • High dielectric strength and stability
  • Low dissipation factor
  • Very good machinability and finishing
  • Available in opaque and transparent grades

RADEL® R series products are targeted at a number of industries and applications. The initial target market is the medical industry. RADEL® R is used in applications for surgical tools and instruments because of its resistance to autoclave sterilization damage. A second market for RADEL® R is electronics because of its temperature resistance and dielectric properties.

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Density 1.29 g/cc0.0466 lb/in³ASTM D792
Water Absorption 0.37 %
@Temperature 22.8 °C,
Time 86400 sec
0.37 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Water Absorption at Saturation 1.1 %
@Temperature 22.8 °C
1.1 %
@Temperature 73.0 °F
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 123123ASTM D785
Tensile Strength, Yield 69.6 MPa
@Temperature 22.8 °C
10100 psi
@Temperature 73.0 °F
ASTM D638
Elongation at Break 60 %
@Temperature 22.8 °C
60 %
@Temperature 73.0 °F
ASTM D638
Tensile Modulus 2.34 GPa340 ksiASTM D638
Flexural Strength 91.0 MPa
@Temperature 22.8 °C
13200 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus 2.41 GPa
@Temperature 22.8 °C
350 ksi
@Temperature 73.0 °F
ASTM D790
Compressive Strength 98.94 MPa14350 psiASTM D695
Izod Impact, Notched 6.94 J/cm
@Temperature 22.8 °C
13.0 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.44
@Frequency 60 Hz,
Temperature 22.8 °C
3.44
@Frequency 60 Hz,
Temperature 73.0 °F
50% RH; ASTM D150
Dielectric Strength 14.2 kV/mm360 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.6 µm/m-°C17.0 µin/in-°FASTM D696
Specific Heat Capacity 1.13 J/g-°C0.270 BTU/lb-°F
Maximum Service Temperature, Air 182 °C360 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 216 °C420 °FASTM D648
Vicat Softening Point 218 °C424 °F
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
BASF Ultrason® E 1010 PES
BASF Ultrason® E 6020 P PES
BASF Ultrason® S 2010 PSU

PENSIN013 / 92830

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.