AMC Mica is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution. The platy nature of AMC Mica contributes to improved crack resistance in formulted, high solids aqueous applications such as joint compound, coating, sealants, and adhesives.Information provided by Imerys |