MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Imerys AMC™ Ground Mica
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: AMC Mica is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution. The platy nature of AMC Mica contributes to improved crack resistance in formulted, high solids aqueous applications such as joint compound, coating, sealants, and adhesives.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.75 g/cc
Bulk Density 22.0 lb/ft³
Density 22.9 lb/gal
Brightness 80 %Whiteness (Hunter L)
Particle Mesh Size 100 Meshless than 0.6% retained
 200 Meshless than 19% retained
 325 Mesh78% through; Alpine Air Jet Sieve
pH 7.9
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 2.5
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.58
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Imerys 325FF™ Ground Mica
Imerys 325D Ground Mica
Imerys PLM 3 Ground Mica
Mica (KAl2(AlSi3O10)(OH)2)
Imerys 160D Ground Mica

CIMERY017 / 88367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.