MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Imerys PLM 3 Ground Mica
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: PLM 3 is a dry Ground Mica (complex potassium aluminum silicate) with a controlled size distribution.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.75 g/cc2.75 g/cc
Bulk Density 0.540 g/cc0.0195 lb/in³
Brightness 80 %80 %Whiteness (Hunter L)
Particle Mesh Size 100 Mesh100 Meshless than 66% retained
 200 Mesh200 Meshless than 27% retained
 200 Mesh200 Mesh15% through; Alpine Air Jet Sieve
pH 7.97.9
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.52.5
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.581.58
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.30 %<= 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Imerys 325FF™ Ground Mica
Aclo Accutech Polypropylene Homopolymer HP0334M10L Mica Reinforced
Aremco Ceramabond™ 632 High Temperature Ceramic Adhesive/Paste, Mica Filled
Mica (KAl2(AlSi3O10)(OH)2)
Imerys 160D Ground Mica

CIMERY021 / 88371

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.