MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Isoflon PEI Polyetherimide
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), Extrusion Grade

Material Notes: Materials with strong mechanical and electrical performances under high temperatures.

Information provided by Isoflon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccDIN 53479
Water Absorption 0.25 %0.25 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 109109ASTM D785
Tensile Strength 105 MPa15200 psiDIN 53455
Elongation at Break 60 %60 %DIN 53455
Tensile Modulus 3.10 GPa450 ksiDIN 53457
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmDIN 53482
Dielectric Constant 3.2
@Frequency 1000 Hz
3.2
@Frequency 1000 Hz
DIN 53483
Dielectric Strength 27.0 - 32.0 kV/mm686 - 813 kV/inDIN 53481
 
Thermal PropertiesMetricEnglishComments
CTE, linear 62.0 µm/m-°C34.4 µin/in-°FDIN 52328
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°FDIN 52612
Melting Point 215 °C419 °FDIN 53736
Maximum Service Temperature, Air 170 °C338 °FContinuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °F
Flammability, UL94 V-0
@Thickness 0.410 mm
V-0
@Thickness 0.0161 in
 
Descriptive Properties
ColorAmber Dark Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hippe PEI
GEHR Plastics PEI Polyetherimide
Overview of materials for Polyetherimide (PEI)
RTP Company RTP 2100 Polyetherimide (PEI)
LNP ULTEM® SMU5834 Polyetherimide, 20% Carbon Fiber Reinforcement

PISOFL929 / 123317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.