MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LNP ULTEM® SMU5834 Polyetherimide, 20% Carbon Fiber Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), Carbon Fiber Filled

Material Notes: High modulus with shielding/ conductive characteristics for high-heat applications.

  • Features: Electrically Conductive, High Heat Resistance, High Strength
  • Forms: Pellets
  • Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 174 MPa25200 psiType I, 5 mm/min; ASTM D638
Elongation at Break 5.0 %5.0 %Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 221 MPa32100 psi(102 mm Span) 3mm/min; ASTM D790
Flexural Modulus 11.7 GPa1700 ksi(102 mm Span) 3mm/min; ASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10000 ohm10000 ohmASTM D257
Static Decay <= 0.010 sec<= 0.010 sec5000V to <50V; FTMS101B
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 212 °C
@Thickness 6.35 mm
414 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 360 - 421 °C680 - 790 °F
Middle Barrel Temperature 371 - 421 °C700 - 790 °F
Front Barrel Temperature 382 - 427 °C720 - 801 °F
Nozzle Temperature 377 - 421 °C711 - 790 °F
Melt Temperature 382 - 427 °C720 - 801 °F
Mold Temperature 135 - 163 °C275 - 325 °F
Drying Temperature 149 °C300 °F
Dry Time <= 24 hour<= 24 hour
Moisture Content 0.020 %0.020 %Suggested
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
Clamp Pressure 41.0 - 69.0 MPa5950 - 10000 psi
Shot Size 40 - 60 %40 - 60 %Suggested
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LNP ULTEM® SMU5806 Polyetherimide, 8% Carbon Fiber Reinforcement
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant
LNP ULTEM® SMU5836 Polyetherimide, 30% Carbon Fiber Reinforcement
Isoflon PEI Polyetherimide
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber

PZLNP1570 / 51652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.