MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MetalTek MTEK B Cast UNS N24030 Nickel-Copper Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Family of alloys for extreme heat and corrosion services.

Applications: Gas Turbine parts. Chemical process equipment, heat treating equipment.

Information provided by MetalTek

Key Words: Cast Grade M-30H; Cast ASTM A494; Military QQ-N-288 Comp B; Wrought UNS N05500; Wrought Grade MONEL® 500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 263263
Tensile Strength, Ultimate >= 690 MPa>= 100000 psi
Tensile Strength, Yield >= 415 MPa>= 60200 psi
Elongation at Break >= 10 %>= 10 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.50 %<= 0.50 %
Carbon, C <= 0.10 %<= 0.10 %
Copper, Cu 27 - 33 %27 - 33 %
Iron, Fe <= 3.5 %<= 3.5 %
Manganese, Mn <= 1.5 %<= 1.5 %
Nickel, Ni 61 - 68 %61 - 68 %
Silicon, Si 2.7 - 3.7 %2.7 - 3.7 %
 
Descriptive Properties
Heat TreatmentNot Heat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals MONEL® Alloy K-500
ATI Allvac® Nickelvac® K-500 UNS N05500 Nickel Superalloy
MetalTek MTEK 20-32Nb Cast UNS N08151 Heat Resistant Stainless Steel
MetalTek MTEK 718 Cast UNS N07718 Severe Corrosion and Heat Resistant Alloy
Special Metals MONEL® Alloy 400

NMETEK139 / 18389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.