MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allvac® Nickelvac® K-500 UNS N05500 Nickel Superalloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Uses: Pump and drive shafts, impellers, valve components, springs, fasteners, oil well packers, subsurface safety valves.

Property values are for samples in the metallurgical condition: 1600°F anneal + water quench + age.

Information provided by Allvac, An Allegheny Teledyne Company.

Key Words: AMS 467. ASTM F 467, F 468.
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.45 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 2727
Tensile Strength, Ultimate 1000 MPa145000 psi
Tensile Strength, Yield 655 MPa
@Strain 0.2 %
95000 psi
@Strain 0.2 %
Elongation at Break 22 %22 %
Reduction of Area 40 %40 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.7 %2.7 %
Carbon, C 0.10 %0.10 %
Copper, Cu 29 %29 %
Iron, Fe 1.0 %1.0 %
Manganese, Mn 0.70 %0.70 %
Nickel, Ni 66 %66 %
Silicon, Si 0.25 %0.25 %
Sulfur, S 0.010 %0.010 %
Tungsten, W 0.60 %0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals MONEL® Alloy K-500
MetalTek MTEK B Cast UNS N24030 Nickel-Copper Alloy
Special Metals INCONEL® Alloy 625
ArcelorMittal Dual Phase 500 Very High Strength Cold Rolled Steel
ATI Allvac® Nickelvac® C 22 UNS N06022 Nickel Superalloy

NALLV01 / 14917

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.