Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 3.40 g/cc | 3.40 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 55 | 55 |
Tensile Strength at Break | 3.45 MPa | 500 psi |
Elongation at Break | >= 200 % | >= 200 % |
Tear Strength | 10.5 kN/m | 59.9 pli |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | >= 1.00e+6 ohm-cm | >= 1.00e+6 ohm-cm |
Surface Resistivity per Square | >= 1.00e+6 ohm | >= 1.00e+6 ohm |
Shielding Effectiveness | -20.0 dB @Thickness 2.36 mm, Frequency 6.80e+9 Hz | -20.0 dB @Thickness 0.0930 in, Frequency 6.80e+9 Hz |
| -17.0 dB @Thickness 0.813 mm, Frequency 1.08e+10 Hz | -17.0 dB @Thickness 0.0320 in, Frequency 1.08e+10 Hz |
| -15.0 dB @Thickness 1.57 mm, Frequency 9.80e+9 Hz | -15.0 dB @Thickness 0.0620 in, Frequency 9.80e+9 Hz |
| -12.0 dB @Thickness 1.57 mm, Frequency 1.08e+10 Hz | -12.0 dB @Thickness 0.0620 in, Frequency 1.08e+10 Hz |
| -12.0 dB @Thickness 2.36 mm, Frequency 4.80e+9 Hz | -12.0 dB @Thickness 0.0930 in, Frequency 4.80e+9 Hz |
| -10.0 dB @Thickness 0.813 mm, Frequency 8.80e+9 Hz | -10.0 dB @Thickness 0.0320 in, Frequency 8.80e+9 Hz |
| -10.0 dB @Thickness 1.57 mm, Frequency 8.80e+9 Hz | -10.0 dB @Thickness 0.0620 in, Frequency 8.80e+9 Hz |
| -10.0 dB @Thickness 3.17 mm, Frequency 2.80e+9 Hz | -10.0 dB @Thickness 0.125 in, Frequency 2.80e+9 Hz |
| -10.0 dB @Thickness 2.36 mm, Frequency 8.80e+9 Hz | -10.0 dB @Thickness 0.0930 in, Frequency 8.80e+9 Hz |
| -8.00 dB @Thickness 1.57 mm, Frequency 6.80e+9 Hz | -8.00 dB @Thickness 0.0620 in, Frequency 6.80e+9 Hz |
| -6.00 dB @Thickness 1.57 mm, Frequency 4.80e+9 Hz | -6.00 dB @Thickness 0.0620 in, Frequency 4.80e+9 Hz |
| -6.00 dB @Thickness 3.17 mm, Frequency 6.80e+9 Hz | -6.00 dB @Thickness 0.125 in, Frequency 6.80e+9 Hz |
| -6.00 dB @Thickness 0.813 mm, Frequency 6.80e+9 Hz | -6.00 dB @Thickness 0.0320 in, Frequency 6.80e+9 Hz |
| -5.00 dB @Thickness 0.508 mm, Frequency 1.08e+10 Hz | -5.00 dB @Thickness 0.0200 in, Frequency 1.08e+10 Hz |
| -5.00 dB @Thickness 2.36 mm, Frequency 1.08e+10 Hz | -5.00 dB @Thickness 0.0930 in, Frequency 1.08e+10 Hz |
| -4.00 dB @Thickness 0.508 mm, Frequency 8.80e+9 Hz | -4.00 dB @Thickness 0.0200 in, Frequency 8.80e+9 Hz |
| -3.00 dB @Thickness 0.813 mm, Frequency 2.80e+9 Hz | -3.00 dB @Thickness 0.0320 in, Frequency 2.80e+9 Hz |
| -3.00 dB @Thickness 0.254 mm, Frequency 1.08e+10 Hz | -3.00 dB @Thickness 0.0100 in, Frequency 1.08e+10 Hz |
| -3.00 dB @Thickness 0.508 mm, Frequency 6.80e+9 Hz | -3.00 dB @Thickness 0.0200 in, Frequency 6.80e+9 Hz |
| -3.00 dB @Thickness 1.57 mm, Frequency 2.80e+9 Hz | -3.00 dB @Thickness 0.0620 in, Frequency 2.80e+9 Hz |
| -3.00 dB @Thickness 2.36 mm, Frequency 2.80e+9 Hz | -3.00 dB @Thickness 0.0930 in, Frequency 2.80e+9 Hz |
| -2.00 dB @Thickness 0.508 mm, Frequency 4.80e+9 Hz | -2.00 dB @Thickness 0.0200 in, Frequency 4.80e+9 Hz |
| -2.00 dB @Thickness 3.17 mm, Frequency 1.08e+10 Hz | -2.00 dB @Thickness 0.125 in, Frequency 1.08e+10 Hz |
| -2.00 dB @Thickness 0.254 mm, Frequency 6.80e+9 Hz | -2.00 dB @Thickness 0.0100 in, Frequency 6.80e+9 Hz |
| -0.500 dB @Thickness 0.254 mm, Frequency 4.80e+9 Hz | -0.500 dB @Thickness 0.0100 in, Frequency 4.80e+9 Hz |
| 0.00 dB @Thickness 0.254 mm, Frequency 8.00e+8 Hz | 0.00 dB @Thickness 0.0100 in, Frequency 8.00e+8 Hz |
| 0.00 dB @Thickness 0.508 mm, Frequency 8.00e+8 Hz | 0.00 dB @Thickness 0.0200 in, Frequency 8.00e+8 Hz |
| 0.00 dB @Thickness 3.17 mm, Frequency 8.00e+8 Hz | 0.00 dB @Thickness 0.125 in, Frequency 8.00e+8 Hz |
| 0.00 dB @Thickness 2.36 mm, Frequency 8.00e+8 Hz | 0.00 dB @Thickness 0.0930 in, Frequency 8.00e+8 Hz |
| 0.00 dB @Thickness 1.57 mm, Frequency 8.00e+8 Hz | 0.00 dB @Thickness 0.0620 in, Frequency 8.00e+8 Hz |
| 0.00 dB @Thickness 0.813 mm, Frequency 8.00e+8 Hz | 0.00 dB @Thickness 0.0320 in, Frequency 8.00e+8 Hz |
|
Thermal Properties | Metric | English | Comments |
---|
Thermal Conductivity | 0.560 W/m-K | 3.89 BTU-in/hr-ft²-°F |
Maximum Service Temperature, Air | 160 °C | 320 °F |
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F |
|
Descriptive Properties |
---|
Composition | Ferrous filled silicone |