MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hong Kun Group UV 123 UV Absorber
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: bis-(1-octyloxy-2,2,6,6-tetramethyl-4-piperidinyl) sebacate;hals hs-112; light stabilizer-123

CAS No.129757-67-1

All information provided by Hongkun Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 5.0 %<= 5.0 %
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  >= 95 %
@Wavelength 425 nm
>= 95 %
@Wavelength 425 nm
 >= 96 %
@Wavelength 450 nm
>= 96 %
@Wavelength 450 nm
 >= 97 %
@Wavelength 500 nm
>= 97 %
@Wavelength 500 nm
 
Descriptive Properties
Appearanceslightly yellow liquid
Purity (%)>= 80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-MUTE 9005 Microwave Absorber
Parker Chomerics CHO-MUTE 9020 RF Absorber
Parker Chomerics CHO-MUTE 9000 Microwave Absorber

PHONGK012 / 86313

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.