MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silberline Sparkle Silvet® 790-30-E1
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final processing by injection molding, extrusion, blow molding or blown film processes. In some cases, Sparkle Silvet® E1 can be used directly in end-use processing but care must be taken to ensure complete dispersion is achieved. Their pellet or granular form make them easy to handle and incorporate.

Applications: Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 47 µm47 µmBefore Conversion
 
Descriptive Properties
% Carrier30
CarrierPolyethylene Wax

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
329 Stainless Steel, annealed pipe
Silberline Silcroma® BG-13
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
Overview of materials for Styrene-Butadiene Copolymer, SBC

ESIBER144 / 5899

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.