MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BCC Products MB 4000 RED Urethane Foundry Plank
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: MB4000 Red is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly shavings, no shrinkage, excellent impact and wear resistance, excellent surface detail reproduction, excellent surface finish, and polishable to a high gloss. Uses: proofing intricate NC designs, numerous tooling aids, various prototypes, architectural models, foundry patterns and core boxes, and short run metal stamping dies.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM-D-792-66
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686ASTM D2240
Tensile Strength, Ultimate 75.08 MPa10890 psi
Elongation at Break 14.5 %14.5 %ASTM D638
Flexural Strength 119.6 MPa17350 psiASTM D790
Flexural Modulus 2.953 GPa428.3 ksiASTM-D-790
Izod Impact, Notched 0.454 J/cm0.850 ft-lb/inASTM D256
Izod Impact Unnotched 29.77 J21.96 ft-lbASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 64.1 µm/m-°C35.6 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FASTM-D-648-56
Glass Transition Temp, Tg 116 °C240 °FASTM D4065

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Reade Advanced Materials Bentonite Powder (BaTiSi3O9)
GEHR Plastics PEEK Polyetheretherketone
Evonik Trogamid® T5002 Nylon 6-3 Compound
Dura-Bar 80-55-06 Continuously Cast Ductile Iron Bar Stock ASTM A536
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536

PBCC013 / 107240

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.