MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dura-Bar 80-55-06 Continuously Cast Ductile Iron Bar Stock ASTM A536
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.

It often is used as a direct replacement for plain carbon steel and can offer dramatic cost reductions for parts that require a lot of machining. The machinability rating of ductile iron bar stock will be similar to free machining carbon steel grades, such as 12L14, 11L17, 86L20, 1141 and 1144, and achievable machining speeds will be significantly higher.

Ductile iron contains graphite in the form of very small, round nodules that give the material free machining properties without the addition of lead, bismuth, sulfur or phosphorus.

The continuous casting process eliminates typical foundry defects, such as gas holes, hard spots, slag inclusions and inconsistent properties, that result from different molding methods. Bars are cast through a water-cooled graphite die mounted on the bottom of a large bar machine crucible. The ferrostatic head pressure created by the molten metal in the bar machine crucible forces iron into the die, producing a very fine-grained microstructure. The outer “rim” is the only part of the bar that is solid when it exits the die. The core is molten iron. Heat from the molten iron core reheats the rapidly chilled outer skin, producing a homogenized microstructure that is cooled to room temperature in still air.

Ductile iron bar stock consists of a microstructure that is made up of graphite nodules in a solid metal matrix. The solid metal matrix will be similar to the matrix structure in carbon steel bars, and the amount of combined carbon determines the mechanical and physical properties of each grade.

The 80-55-06 ductile iron grade has a ferritic/pearlitic matrix. The mechanical properties of 80-55-06 will be similar to medium carbon steels that contain up to 0.50% carbon including 1040, 1045, 1141, and 1144.

All grades of ductile iron bar stock respond very well to conventional heat-treating methods.

Composition: Typical chemical composition and ranges, actual values depend on cross section size.

Information provided by Dura-Bar

Key Words: Nodular iron, ductile iron, Meehanite, spheroidal iron, high strength cast iron, 5506
Vendors: Dura-Bar Metal Services is the leading supplier of Dura-Bar® continuous cast iron and a major distributor of bronze alloys. Our customers rely on us for high quality materials that help increase their profitability. Call us at 1-800-526-0548 or visit dura-barms.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.64 - 7.20 g/cc0.240 - 0.260 lb/in³Approximately 10% lighter than carbon steel
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 187 - 255187 - 255Depends on cast section size and location of test
Tensile Strength, Ultimate 586 MPa85000 psiTypical
Tensile Strength, Yield 400 MPa58000 psiTypical
Elongation at Break 9.0 %9.0 %Typical
Reduction of Area 3.0 %3.0 %
Tensile Modulus 172 GPa25000 ksiTypical
Compressive Yield Strength >= 455 MPa>= 66000 psiCompressive yield is 1.2 times the tensile yield
Poissons Ratio 0.2750.275Generally accepted value
Fatigue Strength 276 MPa
@# of Cycles 1.00e+8
40000 psi
@# of Cycles 1.00e+8
rotating beam
Shear Modulus 67.6 GPa9800 ksicalculated
Shear Strength 496 MPa72000 psiShear strength is 90% of tensile strength for all ductile iron grades
Charpy Impact 20.3 J
@Temperature 23.0 °C
15.0 ft-lb
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000055 ohm-cm0.0000055 ohm-cmAt 2.50% Silicon
Magnetic Permeability 350 - 550350 - 55025 Oersted, Medium hysteresis loss
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 21.0 - 100 °C
6.11 µin/in-°F
@Temperature 69.8 - 212 °F
Mean
 11.9 µm/m-°C
@Temperature 21.0 - 300 °C
6.61 µin/in-°F
@Temperature 69.8 - 572 °F
Mean
 13.4 µm/m-°C
@Temperature 21.0 - 500 °C
7.44 µin/in-°F
@Temperature 69.8 - 932 °F
Mean
 13.7 µm/m-°C
@Temperature 21.0 - 900 °C
7.61 µin/in-°F
@Temperature 69.8 - 1650 °F
Mean
Specific Heat Capacity 0.506 J/g-°C0.121 BTU/lb-°F
Thermal Conductivity 24.2 W/m-K168 BTU-in/hr-ft²-°F
Melting Point 1120 °C2050 °FEutectic temp
Maximum Service Temperature, Air 649 °C1200 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.5 - 3.9 %3.5 - 3.9 %
Chromium, Cr <= 0.050 %<= 0.050 %
Copper, Cu 0.050 - 0.50 %0.050 - 0.50 %
Iron, Fe 95 %95 %
Manganese, Mn 0.15 - 0.35 %0.15 - 0.35 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si 2.25 - 2.75 %2.25 - 2.75 %
Sulfur, S 0.010 - 0.025 %0.010 - 0.025 %
Tin, Sn 0.050 - 0.10 %0.050 - 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1018 Steel, cold drawn
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018
Ductile Iron grade 80-55-06

NDURA02 / 16122

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.