MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Trogamid® T5002 Nylon 6-3 Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6-3 (PA63)

Material Notes: Description: TROGAMID® T compounds are distinguished by the following properties:
  • crystal-clear, optical transparency
  • high mechanical stability
  • high thermostability
  • high viscosity
  • good chemical resistance compared to other plastics
  • good electrical properties
  • low mold shrinkage

The special properties of TROGAMID T have made it useful in many branches of industry:

  • Electrical Industry:
    • high-voltage switch casings
    • cable glands
    • battery seals
    • keys and push buttons
    • terminal strips
    • casings for switches, relays, and counters
    • gearwheels and gear racks
  • Water Resource Management and Filter Technology:
    • filter cups for pneumatic systems
    • filter cups for water treatment
    • fuel filter cups
    • pump casings
    • metering devices
    • inspection glasses
  • Machine and Apparatus Construction:
    • flowmeters
    • liquid-level indicators
    • valve blocks and common control blocks for dispensing and metering equipment
    • guide rails

Specific Notes for this Material: Permanently transparent polyamide with internal mold release agent for injection molding, extrusion, and blow molding

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA 6-3-T, PA NDT/INDT, trimethyl hexamethylene diamine terephthalic acid
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Viscosity Number 125 cm³/g1.25 dl/gISO 307
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686ISO 868
Ball Indentation Hardness 155 MPa22500 psiH30; ISO 2039-1
Tensile Strength, Yield 90.0 MPa13100 psi50 mm/min; ISO 527-1/2
Elongation at Break >= 50 %>= 50 %50 mm/min; ISO 527-1/2
Elongation at Yield 8.0 %8.0 %50 mm/min; ISO 527-1/2
 8.5 %8.5 %5 mm/min, Outer fiber strain at maximum stress; ISO 178
Tensile Modulus 2.80 GPa406 ksiISO 527-1/2
Flexural Strength 104 MPa15100 psi5 mm/min, at 3.5% Strain; ISO 178
 152 MPa22000 psi5 mm/min; ISO 178
Flexural Modulus 3.00 GPa435 ksiISO 178
Charpy Impact Unnotched  NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.900 J/cm²
@Temperature 0.000 °C
4.28 ft-lb/in²
@Temperature 32.0 °F
ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.24 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2500 MPa363000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 1300 MPa189000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
 >= 1.00e+15 ohm>= 1.00e+15 ohmSpec.; IEC 60093
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 50 Hz
4.0
@Frequency 50 Hz
IEC 60250
 4.3
@Frequency 100 Hz
4.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength 26.0 kV/mm660 kV/inK20/P50; IEC 60243-1
Dissipation Factor  0.018
@Frequency 50 Hz
0.018
@Frequency 50 Hz
IEC 60250
 0.026
@Frequency 1e+6 Hz
0.026
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VTest Solution A, 100 drops; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 53.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
29.4 µin/in-°F
@Temperature 73.4 - 176 °F
Longitudinal; ISO 11359
CTE, linear, Transverse to Flow 54.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
30.0 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FISO 75-1/2
Vicat Softening Point 142 °C288 °F50N; ISO 306
 148 °C298 °F10N; ISO 306
Glass Transition Temp, Tg 150 °C302 °FTg, 10 K/min
UL RTI, Mechanical with Impact 80.0 °C
@Thickness 0.800 mm
176 °F
@Thickness 0.0315 in
UL 746 B
UL RTI, Mechanical without Impact 85.0 °C
@Thickness 0.800 mm
185 °F
@Thickness 0.0315 in
UL 746 B
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Glow Wire Test 850 °C
@Thickness 1.00 mm
1560 °F
@Thickness 0.0394 in
IEC 60695-2-1/0-3
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Trogamid® T5000 Nylon 6-3
Evonik Trogamid® T5004 Nylon 6-3 Compound
Evonik TROGAMID® CX9704 Polyamide
Evonik Trogamid® TX7389 Nylon 6-3 Compound
Evonik TROGAMID® CareMX73 Polyamide

PHUK122 / 47256

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.