MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potters Industries Sphericel® 110P8 Hollow Glass Spheres
Categories: Ceramic; Glass; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Sphericel® 110P8 hollow glass spheres displace the same volume of resin as solid spheres of the same size, but are lighter. Using Sphericel® hollow glass spheres, plastics engineers can produce lighter-weight filled parts or use higher density resins without significant increases in part weight. Breakage of these tough hollow spheres is insignificant, they survive injection molding pressures of over 10,000 psi.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Particle Size 4.0 µm4.0 µm10% finer than
 8.0 µm8.0 µm50% finer than
 11.7 µm11.7 µmmean value
 12 - 16 µm12 - 16 µm90% finer than
 
Descriptive Properties
Colorwhite
CompositionBorosilicate Glass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potters Industries Sphericel® 60P18 Hollow Glass Spheres
Mo-Sci Corporation GL-0193 Hollow Glass Spheres
Potters Industries Q-Cel® 7019 Hollow Engineered Glass Microspheres
3M Scotchlite™ S60/10000 Glass Bubbles
Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead

CPOT06 / 1744

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.