MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potters Industries Sphericel® 60P18 Hollow Glass Spheres
Categories: Ceramic; Glass; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: This microsphere is strong with a density of 0.6g/cc, and has the added advantage of a very small particle size of only 18 micron (mean). Fused glass, hollow spheres used as an additive for thermoplastic and thermosetting resin systems.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.600 g/cc0.0217 lb/in³true density of spheres
Particle Size 6.0 - 10 µm6.0 - 10 µm10% finer than
 15 - 19 µm15 - 19 µm50% finer than
 16 - 20 µm16 - 20 µmmean value
 28 - 32 µm28 - 32 µm90% finer than
 
Descriptive Properties
Appearancewhite powder
CompositionFused Inorganic Oxides
Strength (% volume loss)0.111000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potters Industries Sphericel® 110P8 Hollow Glass Spheres
Mercury Sulfide, HgS (Metacinnabarite)
3M Scotch-Weld™ TS115 HGS Polyurethane Reactive Adhesive

CPOT07 / 1745

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.