MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mo-Sci Corporation GL-0193 Hollow Glass Spheres  (discontinued **)
Categories: Ceramic; Glass

Material Notes: Appearance: Hollow microspheres with white color in powder form.

Applications: GL-0193 is a new, low cost, light weight, hollow glass extender for liquid resin systems offering low cost per unit volume displacement. Since GL-0193 displaces 8 to 10 times its weight of conventional mineral fillers, it will reduce the weight and, therefore, the cost of most products. Parts produced with GL-0193 exhibit excellent staple, screw and nail holding power. The low thermal conductivity of GL-0193 also provides excellent thermal insulation for coating systems.

Information provided by Mo-Sci Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.120 g/cc0.00434 lb/in³of Dry Beads
Density 0.170 g/cc0.00614 lb/in³
pH 7.27.2in water
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 8.48 MPa1230 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0519 W/m-K0.360 BTU-in/hr-ft²-°F
Softening Point 980 °C1800 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potters Industries Sphericel® 110P8 Hollow Glass Spheres
Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead
Potters Industries Conduct-O-Fil® SH400S20 Silver-Coated Hollow Glass Spheres
Mo-Sci Corporation GL-0237 Hollow Glass Spheres
Mid-Mountain Materials CERMEX® PR1000-M Premium Grade Thermal Insulation Paper

CMOSCI018 / 137201

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.