MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mueller Alloy 3770 Forging Brass (UNS C37700)
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: General forging applications

Applications: Alloy 3770 is used as rod base stock for press and hammer forgings requiring the excellent corrosion resistance and machinability of brass. Typical applications include valve bodies, hardware, fittings and miscellaneous brass forgings.

Information Provided by Mueller Industries Inc.

Key Words: ASTM B124, UNS C37700, AMS 4614D, SAE J463
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.44 g/cc0.305 lb/in³Based on UNS number
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7878
Tensile Strength at Break 359 MPa52000 psi
Tensile Strength, Yield 138 MPa20000 psi
Elongation at Break 45 %45 %
Machinability 90 %90 %UNS C36000 = 100%
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relieving
Hot-Working Temperature 649 - 704 °C1200 - 1300 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 58 - 61 %58 - 61 %
Iron, Fe <= 0.30 %<= 0.30 %
Lead, Pb 1.5 - 2.5 %1.5 - 2.5 %
Zinc, Zn 36.2 - 40.5 %36.2 - 40.5 %Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Forging Brass, UNS C37700
Architectural Bronze, UNS C38000
Chicago Extruded Metals UNS C37700 Copper-Zinc-Lead Alloy
Architectural Bronze, UNS C38500
High-leaded brass, 62%, UNS C35300

NMUEL903 / 97691

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.